If you can get it bead blasted then the rest is easy. Just mix your chemicals, heat it to 170 to 185 add some steel wool for 30 minutes then put the parts in the solution. Cook for 15 to 20 minutes and then rinse. Dry the parts and soak them in oil and put it back together.
If you have an air compressor you can get a hand held bead blaster for $10. Harbor Freight Tools - Quality Tools at the Lowest Prices
One thing I forgot to mention, don't touch any of the metal parts with your bare fingers after bead blasting. If you do degrease it with acetone before you put it in the solution. Failing to do so will leave nice fingerprints in the parkerizing. :angry::biggrin: